Nitronic

Product Detail

Product Tags

High Temperature Alloy

◆ Nitronic50 (S20910 / XM-19) inonzi nitrogen-enhanced austenitic stainless steel, iyo inonyanya kushandiswa mu petrochemical, textile, food processing and marine industry.

◆Nitronic60 (S21800/Alloy218) ine yakanakisa-yepamusoro-tembiricha oxidation kuramba uye yakaderera-tembiricha inokanganisa kuita, uye inonyanya kushandiswa mune inoshanda anti-kupfeka uye scratch alloy bhiriji mapini uye mamwe mapurojekiti akakosha.

Kemikari yakagadzirwa

Giredhi

C

Si

Mn

S

P

Cr

Ni

Fe

Mo

Ti

Cu

Nb

N

zvimwe

hapana mukuru pane

Nitronic50

0.06

1

4~6

0.03

0.04

20.5 -23.5

11.5–13.5

base

1.5~3

-

-

0.1~0.3

0.2~0.4

-

Nitronic60

0.1

3.5 -4.5

7~9

0.03

0.04

16~18

8~9

base

-

-

-

-

0.08~0.18

-

Alloy pfuma shoma

Giredhi

state

simba rekusimba RmN/m㎡

Goho Simba Rp0.2N/m㎡

Elongation As%

Brinell kuoma HB

Nitronic50

Solution kurapwa

690

380

35

-

Nitronic60

Solution kurapwa

600

320

35

-