Monel 400 Uns N04400 W.Nr. 2.4360 Uye 2.4361
Kuumbwa Kwemakemikari
Alloy | element | C | Si | Mn | S | Ni | Fe | Cu |
Monel 400 | Min | 63.0 | 28.0 | |||||
Max | 0.3 | 0.5 | 2.0 | 0.024 | 2.5 | 34.0 |
Mechanical Properties
Aolly Status | Kusimba simba Rm Mpa Min | Goho simba RP 0. 2 Mpa Min | Elongation A 5 % Min |
Solution | 745 | 325 | 40 |
Zvinhu Zvenyama
Aolly Status | Tensile simba Rm Mpa Min. | Goho simba RP 0. 2 Mpa Min. | Elongation A 5 % |
annealed | 480 | 170 | 35 |
Standard
Tsvimbo, Bar, Waya uye Forging Stock- ASTM B 164 (Rod, Bar, uye Waya), ASTM B 564 (Forgings)
Plate, Sheet uye Strip-,ASTM B 127, ASME SB 127
Pipe & Tube- ASTM B 165(Seamless Pipe neTube), ASTM B 725 (Welded Pipe), ASTM B 730 (Welded Tube), ASTM B 751 (Welded Tube), ASTM B 775 (Welded Pipe), ASTM B 829(Seamless Pipe uye Tube)
Welding Zvigadzirwa- Filler Metal 60-AWS A5.14/ERNiCu-7; Welding Electrode 190-AWS A5.11/ENiCu-7.
Hunhu hweMonel 400
● Kusapinda mumvura yegungwa uye muutsi pakupisa kwakanyanya
● Kupokana kwakanyanya kumvura inoyerera inokurumidza brackish kana mvura yegungwa
● Kuramba kwakanakisa kushushikana nekupwanya kwecorrosion mumvura zhinji yakachena
● Kunyanya kushingirira kune hydrochloric uye hydrofluoric acids kana yakabviswa mweya.
● Inopa kupikisa hydrochloric uye sulfuric acid pane tembiricha ine mwero uye kudzika, asi kashoma zvinhu zvinosarudzwa kune aya asidhi.
● Kunyanya kupikisa kusarerekera uye alkaline munyu
● Kuramba kune chloride kunokonzera kushungurudzika kuora kwekuputika
● Mamichanicha akanaka kubva pasi-zero tembiricha kusvika 1020° F
● Kurwisana kwakanyanya kune alkalis
● Yakapfuura: Alloy N-155
● Zvadaro: Monel k-500 UNS N05500/ W.Nr. 2.4375