Inconel

  • IInconel

    High Temperature Alloy Chemical composition Giredhi C Si Mn SP Cr Ni Fe Al Ti Cu Mo Nb imwe isiri yakakura kupfuura Inconel600 0.15 0.5 0.5 1 0.015 0.03 14~17 base 6~10 - - ≤0.5 - - - Inconel601 0.0 05 10. 25 bas 0.2 0.35 0...