Ikoloy
High Temperature Alloy
◆Incoloy800H (Ns112/N08810), Incoloy800HT, Incoloy800 (Ns111/N08800) zvinhu zvitatu zveiyo yakafanana nickel-iron-chromium alloy series, vane good corrosion resistance, creep resistance and high tembiricha oxidation inoshandiswa mukupisa, kurapwa Kuisa midziyo, yekuvharisa midziyo yekupikisa alloy tubular kudziyisa miviri, kemikari uye petroleum kugadzirisa michina.
◆Incoloy825 (Ns142/N08825) is a general engineering alloy. Iyo ine anti-asidhi uye alkali simbi corrosion kuramba mune zvese oxidizing uye kuderedza nharaunda. Iyo yakakwira nickel yemukati inoita kuti iyo alloy ive neyakagwinya kusagadzikana corrosion kuramba. Inoshandiswa zvakanyanya munzvimbo dzakasiyana dzeindasitiri uko tembiricha yekushanda isingapfuure 550 ° C.
◆Incoloy901 imvura inoomesa, inokambaira inodzivirira kupisa kwesimbi. Iyo alloy ine goho guru uye simba rinogara riri pasi pe650 ° C, yakanaka oxidation resistance iri pasi pe760 ° C, uye yakagadzikana kushandiswa kwenguva refu. Inoshandiswa zvakanyanya mukugadzirwa kwezvikamu zvakaita sezvikamu zvinotenderera zvendege uye pasi gasi turbine injini dzinoshanda pasi pe650 °C.
◆Incoloy925 (N09925) isimbi yealloy ine simba rakanaka remagetsi uye yakawedzera kusagadzikana kwekuora. Inowanzoshandiswa mukugadzirwa kwezvikamu pamafuta uye gasi kuchera #equipment.
◆Incoloy926 is an austenitic stainless steel ine yakafanana chemikemikari yakagadzirwa kune alloy 904L, iyo nitrogen yehuwandu inowedzerwa kusvika inenge 0.2%, uye iyo molybdenum inokwana 6.5%. Inonyanya kushandiswa mumarine engineering, acid gasi nharaunda, flue gasi desulfurization system.
◆Incoloy20 rudzi rwesimbi zvinhu zvinogona kushanda kwenguva yakareba pasi pekushisa kwepamusoro pasi pe600 ℃ uye kumwe kunetseka.
◆Incoloy330 ine simba guru, yakanaka oxidation resistance, corrosion resistance, yakanaka kuneta kusagadzikana, kuputsika kusimba uye zvimwe zvinhu, uye inokodzera simba renyukireya, indasitiri yemakemikari, uye mamwe mashizha emagetsi.
Kemikari yakagadzirwa
Giredhi | C | Si | Mn | S | P | Cr | Ni | Fe | Al | Ti | Cu | Mo | zvimwe |
hapana mukuru pane | |||||||||||||
Incoloy800 | 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19~23 | 30~35 | base | 0.15~0.6 | 0.15~0.6 | ≤0.75 | - | - |
Incoloy800H | 0.05~0.1 | 1 | 1.5 | 0.015 | 0.03 | 19~23 | 30~35 | base | 0.15~0.6 | 0.15~0.6 | ≤0.75 | - | - |
Incoloy800HT | 0.06~0.1 | 1 | 1.5 | 0.015 | 0.03 | 19~23 | 30~35 | base | 0.15~0.6 | 0.15~0.6 | ≤0.75 | - | Al+Ti 0.85~1.2 |
Ikoloy825 | 0.05 | 0.5 | 1 | 0.03 | 0.03 | 19.5–23.5 | 38~46 | base | ≤0.2 | 0.6~1.2 | 1.5~3 | 2.5–3.5 | - |
Incoloy901 | 0.1 | 0.6 | 1 | 0.03 | 0.3 | 11~14 | 40~45 | base | ≤0.35 | 2.35~3.1 | ≤0.5 | 5~7 | Co≤1.0 |
Ikoloy925 | 0.03 | 0.5 | 1 | 0.03 | 0.03 | 19.5–23.5 | 42~46 | base | 0.15~0.5 | 1.9–2.4 | 1.5~3 | 2.5–3.5 | - |
Ikoloy926 | 0.02 | 0.5 | 2 | 0.01 | 0.03 | 19~21 | 24~26 | base | - | - | 0.5~1.5 | 6~7 | N15~0.25 |
Incoloy020 | 0.1 | 0.8 | 0.5 | 0.013 | 0.013 | 23.5 -26.5 | - | 13~16 | ≤1.5 | 0.3~0.7 | ≤0.5 | 2.5–3.7 | - |
Ikoloy330 | 0.04~0.08 | 1~1.5 | 2 | 0.03 | 0.03 | 18~20 | 34~37 | base | - | - | ≤1 | - | - |
Alloy pfuma shoma
Giredhi | state | simba rekusimba RmN/m㎡ | Goho Simba Rp0.2N/m㎡ | Elongation As% | Brinell kuoma HB |
Incoloy800 | Solution kurapwa | 500 | 210 | 35 | - |
Incoloy800H | Solution kurapwa | 450 | 180 | 35 | - |
Incoloy800HT | Solution kurapwa | 500 | 210 | 35 | - |
Ikoloy825 | Solution kurapwa | 500 | 220 | 30 | - |
Incoloy901 | Solution kurapwa | 900 | 550 | 25 | - |
Ikoloy925 | Solution kurapwa | 650 | 300 | 30 | - |
Ikoloy926 | Solution kurapwa | 650 | 295 | 35 | - |
Ikoloy20 | Solution kurapwa | 700 | 300 | 32 | - |
Ikoloy330 | Solution kurapwa | 750 | 310 | 35 | - |