HASTELLOY B2 UNS N10665 W.NR.2.4617
Kuumbwa Kwemakemikari
Alloy | element | C | Si | Mn | S | P | Ni | Cr | Mo | Fe | Co |
Alloy B2 | Min | 26.0 | |||||||||
Max | 0.02 | 0.10 | 1.00 | 0.03 | 0.04 | Balance | 1.0 | 30.0 | 2.0 | 1.0 |
Mechanical Properties
Aolly Status | Kusimba simba Rm Mpa Min | Goho simba RP 0. 2 Mpa Min | Elongation A 5 % Min |
Solution | 745 | 325 | 40 |
Zvinhu Zvenyama
Density g/cm3 | Melting Point ℃ |
9.2 | 1330~1380 |
Standard
Tsvimbo, Bar, Waya uye Forging Stock- ASTM B 335(Rod, Bar), ASTM B 564(Forging),ASTM B 366(Fitting)
Plate, Sheet uye StripASTM B 333
Pipe uye Tube- ASTM B 622(isina musono) ASTM B 619/B626(Welded Tube)
Hunhu hweHastelloy B2
● Kuramba kwakakura kumanikidziro ekupwanya kwegora uye pitting
● Kuramba kwakanyanya pakudzikisa mamiriro akaita sehydrogen chloride, sulfuric, acetic uye phosphoric acids.
● Kuramba kune hydrochloric acid pane zvese zvakadzika uye tembiricha
● Yakapfuura: INCONEL® alloy C-276 UNS N10276/W.Nr. 2.4819
● Zvadaro: HASTELLOY B-3 UNS N10675/W.Nr.2.4600
Sei Tisarudze:
1. Professional R&D timu
Tsigiro yebvunzo yekushandisa inovimbisa kuti hauchanetseki nezve akawanda bvunzo zviridzwa.
2. Kubatana kwekutengesa kwechigadzirwa
Zvigadzirwa zvinotengeswa kunyika dzakawanda pasi rose.
3. Kudzora kwehutano hwakasimba
4. Yakagadzikana nguva yekuendesa uye inonzwisisika kurongeka kwekutora nguva yekudzora.
Isu tiri timu yehunyanzvi, nhengo dzedu dzine makore mazhinji eruzivo mukutengeserana kwenyika. Isu tiri timu yechidiki, izere nekurudziro uye hunyanzvi. Isu tiri timu yakazvipira. Isu tinoshandisa zvigadzirwa zvinogutsa kugutsa vatengi uye kuhwina kuvimba kwavo. Tiri chikwata chine zviroto. Chiroto chedu chakajairika ndechekupa vatengi zvigadzirwa zvakavimbika uye kugadzirisa pamwe chete. Vimba nesu, kukunda-kuhwina.